High temperature resistant silicone strips feel for still images used with sulfur and catalyst will depend on the sulfur content contained in the type of molecule and the amount of diene. Enb-epdm rubber is most likely to have a sulfur removal (or chemical catalyst to decompose sulfur) of about 0.2 to 2.0 parts in addition, if the tire is fixed quickly and steadily at a high height, no substance is used. A single catalyst should be used but several groups of catalysts should be used together, including RAMAAA Seoul Group with the group supplemented with carbamate. This is often the problem found in rubber where EPDM is flowering to the surface. The catalyst in bloom and cut off the amount of catalyst. For the level that doesn't pose a problem.
In addition to common reinforcement sometimes using calcined clay or calcium carbonate as fillers, it causes great many aspects besides will reduce production costs. It also helps to improve the binder county handling as well. Fillers of both types can be easily distributed in gluten tires, are inexpensive, and do not affect the stability of the tire also calcined clay also allows the tire to be fixed at a low water absorption, which is the required attribute. House cables with hard clay are often used as rubber type fillers. Because even this filler helps strengthen the tire. It will speed up the reaction of the tires that will drop.
Epdm rubber and ethylene ratio can be a high point of crystallization. As a result, the strength of the tires is in an unstable state. It can be filled with oil and so on. In some additives the use of more than twice resin (200phr) is considered to be epoch-making rubber, but the sheep ethylene grade is high and its disadvantages are complex. Tires will rubber hard at low temperatures and low temperature performance is bad. Power at lower temperatures also increases tire crystallization speed. Tires soon lose their elasticity. If you want to mix the glue formula for a high capacity filler. You should use hybrid technology inversion (inverted hybrid technology).
Three big car tires are mixed with other rubber. A variety of diene rubber with rubber uses EDPMs of about 30% (by weight) however, to improve the deterioration characteristics due to ozone tire diene most rubber EDPM blends, such as natural rubber INFRARED SBRBR and NBR. Natural rubber tells you that the rubber diene rubber EDPM double bond is less stable and slower, so remove the diene rubber and mix it with asphalt. Epdm rubber strip requires attention to stability.